Author Topic: Can you identify the colours of these beauties?  (Read 1775 times)
0 Members and 1 Guest are viewing this topic.
sam9769
New Forum Member
*
Posts: 12


« on: March 30, 2013, 04:00:49 AM »

Hi,

I bought these beads because I love the colour combination and was wondering if you know what colours have been used?

There are so many different shades of colours and also I have to factor in the different makes of glass that I am totally confused Huh

Can you please help?

https://www.etsy.com/transaction/123626991

Thank you,

Sam.
Logged
Shirley
Forum Member
******
Posts: 831


WWW
« Reply #1 on: March 30, 2013, 04:08:10 AM »

Very pretty beads. The words Vetrofond odds keep jumping into my head, but I could well be wrong. I would guess at Gaia for the blueygreen silver glass.

Have you asked the maker if she will tell you?
Logged

Val Cox Frit - Thai and Bali Silver 
Pauline
Forum Member
****
Posts: 261


happy happy happy


« Reply #2 on: March 30, 2013, 04:11:31 AM »

Possibly effected coral, dark chocolate and apricot yellow for starters.  Are you going to flame off? if so take the beads and compare.  I guarantee everyone near you will try to help!!!
Logged
spexy
Forum Member
***
Posts: 249


« Reply #3 on: March 30, 2013, 05:29:13 AM »

Are you feeling ok Pauline? Effected Coral?
Logged

Pauline
Forum Member
****
Posts: 261


happy happy happy


« Reply #4 on: March 30, 2013, 05:31:27 AM »

Oops, my coral takes after me obviously!!!
Logged
Corinne Lacy
Forum Member
*
Posts: 49


« Reply #5 on: March 30, 2013, 05:58:11 AM »

Oo I might be wrong but doesn't this lampworker use boro glass?? And I know nothing about boro....no doubt someone else will know!!

Corinne

Logged
Redhotsal
Fine Lampwork beads by Sally Carver
Forum Member
******
Posts: 999


Pound Shop Queen


WWW
« Reply #6 on: March 30, 2013, 06:41:21 AM »

Don't think these are borosilicate. It looks like Effetre Coral. There is quite a lot of difference in batches of Coral. In fact - some of the corals that they get in the States are lovely and we don't get them here. There was one batch of Coral which turned out to be a lovely orange and was sold as "tequila sunrise" for a while. Coral gets my vote as it's nice and opaque.
Logged

Krysia@No98
Glass- it's quite literally a part of me
Forum Member
******
Posts: 843



« Reply #7 on: March 30, 2013, 08:06:15 AM »


yup Corel, light red, dark brown, red brown...pastel yellow, possible some middle red in there two juding on the bleeding and I have no idea what the bluey one is.  She does make fantastic beads.

What I recommend is that you make some spacer beads in every colour of glass that you own (label them!) and this will help you when trying to figure out what colours other people are using

Make more then one and etch one of them.  some colours just ping when they are etched.
Logged

-* -  Courage is going from failure to failure with out loosing enthusiasm -*-
Calico Cat
Eldjötnar in training
Forum Member
***
Posts: 198



« Reply #8 on: March 30, 2013, 08:19:03 AM »

I think the bluish colour might be a silver glass -looks as if the surface has a metallic sheen and, if you enlarge the pic, there's a lot of reaction around the dots.

If you are coming to FO, please bring them with you - they are very pretty and we'd all have a great time playing "match the glass"  Grin

Carole
Logged



Watch this space for new Etsy shop . . .
sam9769
New Forum Member
*
Posts: 12


« Reply #9 on: March 30, 2013, 09:05:58 AM »

Hi Guys,

I'll bring them with me to the FO!!


Sam Grin
Logged
Redhotsal
Fine Lampwork beads by Sally Carver
Forum Member
******
Posts: 999


Pound Shop Queen


WWW
« Reply #10 on: March 30, 2013, 11:04:04 AM »

Actually, looking again at the picture that bluey-green colour might be copper green, as there's no fuming around the colours which would suggest that it is a normal glass rather than a silver glass. Also, copper green does go that type of shiny in the kiln.
Logged

Krysia@No98
Glass- it's quite literally a part of me
Forum Member
******
Posts: 843



« Reply #11 on: March 31, 2013, 04:56:30 AM »


hummm....  I'm going to get out a rod of copper green to play with this afternoon....
Logged

-* -  Courage is going from failure to failure with out loosing enthusiasm -*-