Author Topic: How much frit?  (Read 1789 times)
0 Members and 1 Guest are viewing this topic.
anditsinthefish
Forum Member
***
Posts: 138



« on: January 12, 2013, 08:38:26 AM »

I am trying to work out some prices and figures for my business plan. I was just wondered if anyone knew on average, how much frit on bead uses when rolled in it? Or how many beads you get out of say a 25g bag? Smiley Thanks xx
Logged

Sarah xx
Website. Blog. Flickr.
Helen G
Helen
Forum Member
****
Posts: 367


RIP Doris 31/10/2011


WWW
« Reply #1 on: January 12, 2013, 04:01:46 PM »

It's a bit like asking how long is a piece of string! Depends on how big the beads are and what look you want to achieve.
Logged

Margram
Temperature's rising
Forum Member
*****
Posts: 712


Glass in pocket


« Reply #2 on: January 13, 2013, 04:24:31 AM »

Easiest way would be to weigh out a gram of frit and see how many average-sized beads you get out of it...then multiply by 25! Smiley
Logged

SueP
Forum Member
***
Posts: 247



WWW
« Reply #3 on: January 14, 2013, 04:22:47 PM »

Or if you roll the beads in a "spoonful" of frit put all 25 g in your usual receptacle make a set number of beads then weigh the left over frit to work out how much you have used then divide by number of beads made  Grin
Logged

mizgeorge
Administrator
*******
Posts: 801


Or should that be missus?


WWW
« Reply #4 on: January 14, 2013, 06:04:01 PM »

And don't forget to allow for all the frit you spill onto the floor, pour into your lap, and muddle up with another blend by accident.....
Logged

Fiona
Forum Member
***
Posts: 128


WWW
« Reply #5 on: January 14, 2013, 06:25:52 PM »

You could weigh an average size bead and assuming the 5% rule of applying frit to a bead work out how much that weighs. Maybe up it to 10% to allow for spillage, etc.
Logged