Frit-Happens !
July 05, 2020, 01:26:52 AM *
Welcome, Guest. Please login or register.

Login with username, password and session length
your ad here
News:
Where are you?? Add yourself to the NEW FHF map here  | On flickr? Join our Frit Happens group: here

VISIT THE WIKI HERE
Get FH Status updates via twitter @FritHappens

 
   Home   Help Search Calendar Login Register  
Pages: [1]
  Print  
Author Topic: Bullseye Glass App for iPhone  (Read 1896 times)
0 Members and 1 Guest are viewing this topic.
Zeldazog
My name's Dawn, I'm an
Administrator
*******
Posts: 1048


I'm free, to do what I want...♪♪♪


« on: November 06, 2012, 10:43:36 AM »

Came across this the other day, an app for iPhone etc.

http://www.bullseyeglass.com/index.php?option=com_jfusion&Itemid=224&jfile=viewtopic.php&f=14&t=3367

Contains all the tech notes, a temp/rate converter, annealing calculators for thicker slabs, and has the catalogue.  Doesn't look like it's available for android yet, but hopefully will be sometime. 

Logged

noora
Glassy Swede
Forum Member
***
Posts: 241



« Reply #1 on: November 06, 2012, 03:16:53 PM »

Ooh, shiny  Cheesy I hope it works on my antique iphone 3G. I've found that more and more apps require a newer iOS than what's available for the original 3G Sad
Logged
sparrow
I hold with those who favor fire.
Senior Forum Member
*
Posts: 869


I'm working on a dream...


WWW
« Reply #2 on: November 06, 2012, 03:27:52 PM »

Nice one, Dawn, thank you!
Logged

Zeldazog
My name's Dawn, I'm an
Administrator
*******
Posts: 1048


I'm free, to do what I want...♪♪♪


« Reply #3 on: November 06, 2012, 03:31:48 PM »

Ooh, shiny  Cheesy I hope it works on my antique iphone 3G. I've found that more and more apps require a newer iOS than what's available for the original 3G Sad

Says requires iOs 4.3 or higher...
Logged

julieHB
Global Moderator
*******
Posts: 887



WWW
« Reply #4 on: November 06, 2012, 03:56:39 PM »

You tease, Dawn (Android here....)  Cheesy
Logged

Julie xx

                            My Webbie - My Flickr
sparrow
I hold with those who favor fire.
Senior Forum Member
*
Posts: 869


I'm working on a dream...


WWW
« Reply #5 on: November 06, 2012, 03:58:29 PM »

The annealing calculator looks faaaaab....wish I'd had this *before* the pigeons!
Logged

mariag
Talent is a flame. Genius is a fire
Forum Member
***
Posts: 110


Mia Glass Art


« Reply #6 on: November 06, 2012, 05:14:07 PM »

Ooooooh, it uploads on the iPad too Grin
Thanks Dawn.
Logged

noora
Glassy Swede
Forum Member
***
Posts: 241



« Reply #7 on: November 07, 2012, 01:55:19 AM »

Ooh, shiny  Cheesy I hope it works on my antique iphone 3G. I've found that more and more apps require a newer iOS than what's available for the original 3G Sad

Says requires iOs 4.3 or higher...


Typical, my phone has 4.2 and won't support any newer OS :-( I guess this is Apples way of forcing me to buy a new phone even though my old phone still works perfectly  Angry
Logged
Calico Cat
Eldjötnar in training
Forum Member
***
Posts: 198



« Reply #8 on: November 07, 2012, 02:13:35 AM »

Thank you - works fine on an iPad  Grin
Logged



Watch this space for new Etsy shop . . .
Flyingcheesetoastie
On Golden Wings of Cheddar...
Forum Member
****
Posts: 361


Mostly making glass...


WWW
« Reply #9 on: November 07, 2012, 04:23:04 AM »

I've had this app for a while and it's a good starting point for things. I'm not sure the annealing allows for molds as well as glass though.