Opening a hobby fuser

Started by jeannette, July 31, 2012, 10:23:48 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

jeannette

Aside from "very carefully" how do you open a hobbyfuser to peek inside?
<Looks hopefully>

Melty

I've opened mine at various stages and had no issues - I just lift the lid (carefully) and look in ... obviously don't open it too wide or keep it open for too long ...
Bertie

Melty

This post has lots of good tips - from people who know much more than me :D
Bertie

jeannette

Do you get a hot blast when you open it?

Flyingcheesetoastie

I'm actually opening my top loader kiln at the moment to charge a large cast I've got in there. It's so big that there's no other way to fill it with the glass it needs so have a steel container for the glass, hi temp kevlar gloves up to elbows and an eye firmly fixed on the controller temp. Although at 900c the drop as I open the lid isn't a big issue.