MyPrecious
Forum Member
****
Posts: 277



WWW
« Reply #15 on: July 16, 2012, 03:23:54 PM »

No problem! The hardest bit was taking the pictures, as you can see with all the blurry ones there are! Cheesy

Now I want to see everyone making florals! Flowers everywhere! Wink  Tongue
Logged

GaysieMay
I think, therefore I worry!
Forum Member
*****
Posts: 553


The hair is always in need of taming!


WWW
« Reply #16 on: July 17, 2012, 02:20:26 AM »

Beautifully clear Kathy - thank you for doing that!  Kiss Kiss Kiss
Logged

elliot
New Forum Member
*
Posts: 4


WWW
« Reply #17 on: July 17, 2012, 02:39:10 AM »

 Cool thank you for that! Although I'm a beginner I'll give it a go, it looks so nice on the pictures  Smiley
Logged

LilLizaJane
Forum Member
***
Posts: 111

Only slightly scorched so far ...


WWW
« Reply #18 on: July 17, 2012, 09:41:01 AM »

Awwww, Kathy - you're a godsend! That's so kind and so very, very helpful!
Now I know what I'll be attempting this evening ....
Logged

maintaining eccentricity in the midst of madness
www.LilLizaJane.etsy.com.  (aka Beth)
Andy Davies
Forum Member
**
Posts: 58



« Reply #19 on: January 06, 2014, 11:26:00 AM »

Thank you for posting this, I'm brand-new to the hobby and haven’t even read a book on the topic so this is going to be a big help.
I’ve got about 130 glass rods that I bought 15 years ago, (25 colours) but it’s only the last couple of days that I got a Hot-Head. I was going to make a screen with the rods, just stacking them side by side in a wooden frame but I think a bit of lamp work is going to be a bit more challenging.
Thanks again.

           Kind Regards ... Andy   
Logged

Andy Davies
MyPrecious
Forum Member
****
Posts: 277



WWW
« Reply #20 on: January 06, 2014, 04:37:26 PM »

You're welcome! Wink Have fun!
Logged

lantana
Forum Member
**
Posts: 66

Goodness gracious, small balls of fire!


WWW
« Reply #21 on: January 07, 2014, 09:36:07 AM »

Great mini tutorial, it's really kind of you the share it Smiley
Logged
Pauline
Forum Member
****
Posts: 271


happy happy happy


« Reply #22 on: January 07, 2014, 04:15:26 PM »

thats great, thank you
Logged
jeannette
Forum Member
***
Posts: 172


WWW
« Reply #23 on: January 07, 2014, 05:01:51 PM »

Oh thanks, I kind of tried this without advice just guessing and I can see where I went wrong! Kewl!