jeannette

You know I did wonder if there was some reaction between the glasses...
Glad it's "just" my bad luck :)

GlassOwl

Looks great

First piece I ever made I picked a white piece of glass which struck salmon pink, made something I was creating look really weird but I still love it.

Best thing to do is mark it in some way,  :) but it looks like a happy accident.

Have fun with the student pack, I still have loads of bits from my dichro student pack and that can create many interesting accidents as well