Avril
New Forum Member
*
Posts: 10


I will do it !!!


« on: June 28, 2012, 02:21:59 PM »

I would be really interested to know what type of glass people prefer to use for encasing and if there is any glass that should be avoided?
Thanx  Huh
Logged
Dragonfire Glass
Forum Member
*****
Posts: 597



WWW
« Reply #1 on: June 28, 2012, 04:31:13 PM »

I use 006 most of the time, zephyr is gorgeous but with a price tag.
Logged

Redhotsal
Fine Lampwork beads by Sally Carver
Forum Member
******
Posts: 999


Pound Shop Queen


WWW
« Reply #2 on: June 28, 2012, 04:46:30 PM »

The current batch of Effetre 006  is great. Avoid Effetre 004, it tends to scum. CIM clear is nice. Never tried Zephyr but woudln't buy it because of the HUGE price tag.
Logged

BeeBeads
Forum Member
****
Posts: 335

Still here!


« Reply #3 on: June 29, 2012, 03:45:21 AM »

I like 006 too .. never used Zephyr because of the huge price tag.  But you'll probably get loads of replies from those who do use it!
Logged
Helen G
Helen
Forum Member
****
Posts: 367


RIP Doris 31/10/2011


WWW
« Reply #4 on: June 29, 2012, 06:43:54 AM »

006 for me too, Zephyr is good but I can't justify the expense as I use LOTS of clear in my beads  Wink
Logged

♥♥Tan♥♥
cuntbuckets
Forum Member
*******
Posts: 1300



WWW
« Reply #5 on: June 29, 2012, 07:06:00 AM »

Steer clear of vetrofond, I have an old batch that hazes every time it is heated and blackens really easily. Effetre seems to be a good all rounder.
Logged

ScarletLeonard
or Scarlett, or Scarlette
Forum Member
****
Posts: 424



WWW
« Reply #6 on: June 29, 2012, 07:09:16 AM »

006.

CiM clear is fine on a minor but not on a HH.
Logged

GaysieMay
I think, therefore I worry!
Forum Member
*****
Posts: 553


The hair is always in need of taming!


WWW
« Reply #7 on: June 29, 2012, 10:01:03 AM »

I like reichenbach soft crystal, or 006 effetre - I'm on the reichenbach at the moment and zephr for special beads!  Smiley
Logged

Avril
New Forum Member
*
Posts: 10


I will do it !!!


« Reply #8 on: June 29, 2012, 11:55:28 AM »

Thank you all.  I am trying some Lauscha at the moment that George kindly gave to me to try but I think I might just order some of the 006 and Reichenbach to compare them.   Grin
Logged
Blue Box Studio
Blue sky thinking & a load of hot air
Forum Member
******
Posts: 963


Just give me the coffee and no one gets hurt!


WWW
« Reply #9 on: June 29, 2012, 12:13:40 PM »

006 for me - but since DH helped sort the glass and put all the colours (including clear) together, I often use 004 (best for something not seen) Cim or Vetrofond by mistake.  But scum and cloudiness usually sorts one rod from the rest.
Logged

MyPrecious
Forum Member
****
Posts: 277



WWW
« Reply #10 on: June 29, 2012, 01:02:50 PM »

Effetre 006 at the moment for me, but I had no problem using Vetrofond a few years ago.
Logged

Helen G
Helen
Forum Member
****
Posts: 367


RIP Doris 31/10/2011


WWW
« Reply #11 on: July 02, 2012, 10:07:18 AM »

Effetre 006 at the moment for me, but I had no problem using Vetrofond a few years ago.

Me too! I must have had an amazing batch, I bought a kilo of it but when I ran out the replacement was horrible Sad
Logged

Mand
Mandmade - that's me.
Forum Member
****
Posts: 295


Go f'rit! (80's me)


WWW
« Reply #12 on: July 02, 2012, 10:18:40 AM »

006 for me too.  Scarlet - I've always found that CiM clear makes my beads crack for some strange reason  ....