Author Topic: Disc Beads  (Read 2382 times)
0 Members and 1 Guest are viewing this topic.
chipperpottery
Life passes by when melting glass.
Forum Member
****
Posts: 370


WWW
« on: June 26, 2012, 06:22:34 AM »

Any advise on how to make disc beads please.
I have a multi shaper, had it ages, but never tried out the disc shape until this morning.
Found it difficult to get a nice round disc ??
Logged

Krysia@No98
Glass- it's quite literally a part of me
Forum Member
******
Posts: 843



« Reply #1 on: June 26, 2012, 09:21:26 AM »


Is that the one where there are five shapes in one?  If so that's the same one I have and I have not worked out how to used it.  I have a feeling that I will 'get it' after I've played around with the bigger ones.  (On my list to buy at the flame off next year)

I think it's too small to learn on.  I would say though that the most successful ones I have made so far have been when I have made a little bead and then slowly layered it up.  I would say also that it would be good to have something to take excess glass of with
Logged

-* -  Courage is going from failure to failure with out loosing enthusiasm -*-
Blue Box Studio
Blue sky thinking & a load of hot air
Forum Member
******
Posts: 963


Just give me the coffee and no one gets hurt!


WWW
« Reply #2 on: June 26, 2012, 09:23:57 AM »

Multishaper?  Is there a tool I've missed?

Logged

suzielaws
Forum Member
**
Posts: 79


Feeling grey put on a bead to brighten your day!


WWW
« Reply #3 on: June 26, 2012, 09:26:15 AM »

Make the base bead to fit the cavity and then just add layer by layer rolling as you go and adding glass where you need it. It is tricky though and the smaller the disk i find it harder.
Logged

Krysia@No98
Glass- it's quite literally a part of me
Forum Member
******
Posts: 843



« Reply #4 on: June 26, 2012, 09:46:01 AM »

Multishaper?  Is there a tool I've missed?

It's a bead roller for the indecisive  Wink  It has 5 shapes.  So far I have mastered one, the round one  Roll Eyes 
Logged

-* -  Courage is going from failure to failure with out loosing enthusiasm -*-
Kaz
Flame Off Show Off
Senior Forum Member
*
Posts: 1251


Worth my weight in glass....


WWW
« Reply #5 on: June 26, 2012, 12:50:30 PM »

Make the base bead to fit the cavity and then just add layer by layer rolling as you go and adding glass where you need it. It is tricky though and the smaller the disk i find it harder.
Exactly wot she said!
Logged

She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!
chipperpottery
Life passes by when melting glass.
Forum Member
****
Posts: 370


WWW
« Reply #6 on: June 26, 2012, 01:15:03 PM »

Thanks everyone.
Logged

flowerjasper
Forum Member
****
Posts: 470


Acorns!


WWW
« Reply #7 on: June 26, 2012, 02:43:07 PM »

Make the base bead to fit the cavity and then just add layer by layer rolling as you go and adding glass where you need it. It is tricky though and the smaller the disk i find it harder.
Exactly wot she said!
I echo that, I have one of the multi shapers, a four sided brass one, with a different shape on each side, I couldnt get the disc shape at all, untill one day I did as above,  putting small amounts of glass and pulling stringers to get just a little glass to finish off,

sandy
Logged

GaysieMay
I think, therefore I worry!
Forum Member
*****
Posts: 553


The hair is always in need of taming!


WWW
« Reply #8 on: June 26, 2012, 03:33:44 PM »

They are gorgeous Sandy - I love your colour choice. x
Logged

flowerjasper
Forum Member
****
Posts: 470


Acorns!


WWW
« Reply #9 on: June 26, 2012, 04:47:03 PM »

thank you ,
i have always loved purple and green
petrol green,  a reichenbach purple (think its opaque lilac), pea green and light torquoise.
Discs are a great way of getting good colour combos  Grin
sandy x
Logged

Margram
Temperature's rising
Forum Member
*****
Posts: 690


Glass in pocket


« Reply #10 on: June 27, 2012, 03:23:06 PM »

Mmmm, I want to put my hand into the screen and nab them! Smiley
Logged