chipperpottery
Life passes by when melting glass.
Forum Member
****
Posts: 370


WWW
« on: June 08, 2012, 10:19:16 AM »

O'k I am fed up with pricking my fingers with my reamer, when cleaning out my bead holes.
What do you all use?
Is there an electric or batter operated reamer.
Logged

lampworklover
yes, I managed to change my pic, only took 3 years
Forum Member
***
Posts: 234



WWW
« Reply #1 on: June 08, 2012, 10:41:34 AM »

I bought an electric reamer from martin, 'tis brilliant  Cheesy
Logged

Blue Box Studio
Blue sky thinking & a load of hot air
Forum Member
******
Posts: 963


Just give me the coffee and no one gets hurt!


WWW
« Reply #2 on: June 08, 2012, 11:06:49 AM »

Is it better than the battery one Martin sells?  There aren't replacement bits for the battery one and my last one has been problematic.
Logged

lampworklover
yes, I managed to change my pic, only took 3 years
Forum Member
***
Posts: 234



WWW
« Reply #3 on: June 08, 2012, 11:39:13 AM »

Noty seen the battery one, but you can def get replacement bits for the electric one.
Logged

Madam Steph
Forum Member
****
Posts: 440


Jon Snow just CAN'T be dead!


WWW
« Reply #4 on: June 08, 2012, 11:40:24 AM »

This is uncanny!
For 2 days solid now, I have been racking my brains trying to remember where to get those rather expensive reamers that were mentioned on here some months back.
I think Kathy said that she uses them, and as is my usual way, I never got around to actually buying some.
I really wish that Martin would find a way to stock the thinner of the three reamers that come with the battery operated one that he sells, as since I started using 2mm mandrels, only the thinner one for 1.6mm mandrels fits.

I haven't seen the electric ones that Martin sells. I'll have to go look now

Linda x
Logged

Lakelady
TurnerRoweGlassArt
Forum Member
****
Posts: 357


Shakin that gl ass!


WWW
« Reply #5 on: June 08, 2012, 11:49:55 AM »

I have stabbed myself countless times too Rita.  Have heard mention of the electric ones from Martin on here before but never found them on the site!
Logged

Turner Rowe Glass Art
flame n fuse
Forum Member
****
Posts: 464


WWW
« Reply #6 on: June 08, 2012, 12:52:44 PM »

If I only have a few beads to do, I use a mandrel of the appropriate size, dipped while damp into silicon carbide grit from Mango beads - works a treat!
Logged
BeeBeads
Forum Member
****
Posts: 300

Still here!


« Reply #7 on: June 08, 2012, 12:56:13 PM »

I use the grits as well, with a mandrel or a hand reamer.  They work very well.  I got mine from Jocks years ago.
Logged
Blue Box Studio
Blue sky thinking & a load of hot air
Forum Member
******
Posts: 963


Just give me the coffee and no one gets hurt!


WWW
« Reply #8 on: June 08, 2012, 01:01:33 PM »

Can only see the manual reamer on Martin's website now?
Logged

Madam Steph
Forum Member
****
Posts: 440


Jon Snow just CAN'T be dead!


WWW
« Reply #9 on: June 08, 2012, 02:38:16 PM »

The grit is fantastic. I use it on'see-throughs'.

Linda x
Logged

Trudi
Forum Member
*******
Posts: 1674


This is me!


WWW
« Reply #10 on: June 08, 2012, 03:23:37 PM »

I bought a rotary tool From eBay, works a treat
Logged

Glyn Burton
Forum Member
***
Posts: 149


WWW
« Reply #11 on: June 08, 2012, 03:47:21 PM »

if you have a lot to do buy a pedant drill from axminster with some diamond burrs. Worth the initial outlay you can use the pendant drill for engraving, polishing grinding and cutting its a worthwhile addition to your workshop.
The axminster code for the tool is 300228 and the handset 910340.
« Last Edit: June 08, 2012, 04:07:59 PM by Glyn Burton » Logged
Miriam
Forum Member
**
Posts: 65



WWW
« Reply #12 on: June 08, 2012, 11:48:36 PM »

I use a cordless Dremel with a diamond bit from Artintheround. The tip has no grid on it, so if you are not good at aiming for the hole, you won't scratch your bead.
Logged

groetjes Miriam


Blog | Website | Colorcharts | Glasss
Pat from Canvey
Only a little bit odd
Forum Member
*******
Posts: 1222


Keep on blowing


« Reply #13 on: June 09, 2012, 04:46:12 AM »

Re aiming for the bead hole, I lightly insert the tip into the bead hole before turning the drill on.
Logged

Madam Steph
Forum Member
****
Posts: 440


Jon Snow just CAN'T be dead!


WWW
« Reply #14 on: June 09, 2012, 05:02:12 AM »

Thanks, Miriam.
That was the reamer I couldn't find again

Linda x