binty
I likes meltin stuff, I do
Forum Member
**
Posts: 72



« on: June 05, 2012, 06:09:00 PM »

I had a little go at a slinky bracelet, I'm really pleased at how it turned out

Untitled by binty13, on Flickr



Untitled by binty13, on Flickr
Logged
Glassy Lou
Melter of glass and fingers
Forum Member
***
Posts: 187


« Reply #1 on: June 05, 2012, 11:17:47 PM »

That's lovely  Smiley
Logged

Pat from Canvey
Only a little bit odd
Forum Member
*******
Posts: 1222


Keep on blowing


« Reply #2 on: June 06, 2012, 02:09:44 AM »

So you should be. It's lovely.
Logged

GaysieMay
I think, therefore I worry!
Forum Member
*****
Posts: 553


The hair is always in need of taming!


WWW
« Reply #3 on: June 06, 2012, 04:23:27 AM »

Very elegant!  I love the colours you've used as well. x
Logged

justjules
Forum Member
**
Posts: 64



« Reply #4 on: June 06, 2012, 04:48:49 AM »

really nice Lisa, I love the Toho triangles
 Smiley
Logged
Lotti
Blond and bonkers
Forum Member
*****
Posts: 537


Let me at that torch!


WWW
« Reply #5 on: June 06, 2012, 05:15:49 AM »

Wow, I love that. Smiley  So envious of folks who have the patience (and eyesight) to play with seed beads, I used to but just can't anymore and never something as fab as this. Smiley Smiley
Logged

binty
I likes meltin stuff, I do
Forum Member
**
Posts: 72



« Reply #6 on: June 06, 2012, 05:21:16 AM »

Thank you. Jules I was inspired by all your lovely thinks at flame off, I've had the kit sitting there for about 3 years!!  It was quite simple once I got my head around it, took me about 4 hours but I am very slooooooow!!
Logged
Margram
Temperature's rising
Forum Member
*****
Posts: 697


Glass in pocket


« Reply #7 on: June 06, 2012, 05:57:45 PM »

Very nice! Smiley
Logged

MyPrecious
Forum Member
****
Posts: 277



WWW
« Reply #8 on: June 07, 2012, 02:14:32 AM »

I love it! Smiley
Logged

nuttybeader
Forum Member
**
Posts: 66



« Reply #9 on: July 05, 2012, 10:48:23 AM »

It's lovely.
Logged
BeeBeads
Forum Member
****
Posts: 342

Still here!


« Reply #10 on: July 05, 2012, 10:59:34 AM »

Gorgeous, very glam!   Grin
Logged
justjules
Forum Member
**
Posts: 64



« Reply #11 on: July 05, 2012, 11:37:54 AM »

Thank you. Jules I was inspired by all your lovely thinks at flame off, I've had the kit sitting there for about 3 years!!  It was quite simple once I got my head around it, took me about 4 hours but I am very slooooooow!!
you'll get faster. The first time I do a new design it always takes much longer than subsequent attempts

 Smiley
Logged
Rascal
Forum Member
***
Posts: 188


« Reply #12 on: July 05, 2012, 03:23:16 PM »

That looks great, I'd end up playing with it on my wrist as it looks really satisfying to fiddle with. Perhaps you could market it as a stress relief bracelet or to help people cope with boredom in meetings  Grin