what do you put your frit on??

Started by Pauline, March 18, 2012, 07:45:42 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

the lady with the lamp

 :D Ive got a brass off cut with the middle rounded out and when ive finished i use a tiny funnel to put the leftover frit back,it makes it very easy to tidy-up.

ScarletLeonard

Like Colette I use folded up tinfoil.

Les

I've made frit dishes out of the bottom of coke cans ... I'll post a pic if you like tomorrow ... they're just perfect for the job :)

Pauline

Quote from: Les on March 18, 2012, 10:17:38 PM
I've made frit dishes out of the bottom of coke cans ... I'll post a pic if you like tomorrow ... they're just perfect for the job :)

yes please :D

Les


Blue Box Studio

Quote from: the lady with the lamp on March 18, 2012, 10:01:19 PM
:D Ive got a brass off cut with the middle rounded out and when ive finished i use a tiny funnel to put the leftover frit back,it makes it very easy to tidy-up.

Oh yes, a funnel.  I'd get it everywhere without the funnel - courtesy of a Tupperware raffle years ago.
Sue
Website ~ Etsy ~ Blog ~ Flickr

Margram

A soup spoon held over a metal gravy boat - I push the frit right up to the edge of the spoon and if any falls off it is easy to pour back into the frit container :)
Marg x  Etsy Flickr My blog

MyPrecious

I like to use the back of my beadrollers or the bottom part of the lentil press.
Kathy

My website

Kaz

I'm a sprinkler. I put the frit in a bowl under the flame and use a melon baller or teaspoon to sprinkle the frit over the heated bead. I have a teeny steel funnel for putting the frit back into its container.
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Pat from Canvey

I use a small mainly flat, brass swan I found in a charity shop. The pointed tail lets me pour the frit back in it's tub. I like the coke can bottom tip though.

sarah t

if using a bead press i use the press  otherwise back of a bead roller,marver ,foil dish in fact anything handy

you can use your foil 'ashtrays' for all kinds of things things ,i have murrini keeping warm on my kiln in a few

GlassOcean

I have got fondue spoons, from a charity shop, I use them every time I make beads, they are fab!

fionaess



If it's got a hole, it's a bead !

helbels

What an inventive lot we are!!! Who'd have thought that so many ingenious solutions could be devised for such a simple problem! :D :D

Les

Here's those trays ... I took a close up so you can see how they're made :)


DIY Frit Tray by Mad Cat Glass, on Flickr