Author Topic: From Tongue Pink to Striking Terracotta  (Read 4356 times)
0 Members and 1 Guest are viewing this topic.
Lush!
Julie
Forum Member
*******
Posts: 1145


Queen of Buttons :0)


WWW
« on: July 10, 2011, 05:45:25 PM »

http://juliefountain.blogspot.com/2011/07/striking-terracotta.html

 Grin Grin
Logged

Hazel
Forum Member
*
Posts: 37


« Reply #1 on: July 10, 2011, 06:18:05 PM »

Thankyou so much for sharing that with us all Julie, you make it look so easy!
I've just had a play with TP and silver wire - I can't wait to see the results in the kiln tomorrow mornig.
Hazel
Logged

rocky
is waiting for inspiration ......
Forum Member
**
Posts: 98



« Reply #2 on: July 10, 2011, 06:29:17 PM »

Awesome instruction Smiley I might just have a play ....

Thankyou Smiley
Logged

Deanne x
Rainbow1
Forum Member
*
Posts: 40



« Reply #3 on: July 11, 2011, 05:44:15 AM »

Thanks so much Julie, you have inspired me to go have a play when I get home from work Grin
Logged

Jo x
febgirl
New Forum Member
*
Posts: 10



« Reply #4 on: July 11, 2011, 07:26:34 AM »

Thank you Julie:) going home to have a go.
Logged

Caroline
xx
Ant
Forum Member
**
Posts: 58


What doesn't kill me makes me stronger!


WWW
« Reply #5 on: July 11, 2011, 06:06:42 PM »

So Julie, does the TP actually need silver to strike then?  Is it not possible to strike it on its own?  I got some with my Tuffnell's order last week and will have a play soon - but too hot for me this evening!
Logged

Lush!
Julie
Forum Member
*******
Posts: 1145


Queen of Buttons :0)


WWW
« Reply #6 on: July 11, 2011, 06:09:48 PM »

Hmm, that's a good question actually, Anthea.  I shall have to investigate ...
Logged

Alison G
Forum Member
***
Posts: 142


Buys Beads Regardless - My First Nations name.


« Reply #7 on: July 11, 2011, 06:14:28 PM »

*coughs* I've had it strike on it's own. Mainly because I thought that's what you did  Roll Eyes and haven't tried silver with it.

Rapid cooling, like with a press, seems to help.

(sorry to hijack Mrs F!)
Logged

NB. Do not touch hot rods of glass, it is stupid.
Lush!
Julie
Forum Member
*******
Posts: 1145


Queen of Buttons :0)


WWW
« Reply #8 on: July 11, 2011, 06:16:39 PM »

Not at all, Mrs G, its good to know  Grin
Logged

Shirl
Forum Member
****
Posts: 371


« Reply #9 on: July 11, 2011, 06:23:38 PM »

So Julie, does the TP actually need silver to strike then?  Is it not possible to strike it on its own?  I got some with my Tuffnell's order last week and will have a play soon - but too hot for me this evening!

I made some plain TP beads tonight, they are in the kiln and they struck without any silver Smiley
Logged

flaming beads
Forum Member
**
Posts: 77


WWW
« Reply #10 on: July 12, 2011, 04:35:27 AM »

Another brilliant write up Julie...thankyou Grin
I've struck TP without silver before!
Logged
dangerousbead
Forum Member
***
Posts: 205



WWW
« Reply #11 on: July 12, 2011, 07:28:31 AM »

Thanks for doing that, I'm book marking your blog from now on.
Logged
Shirl
Forum Member
****
Posts: 371


« Reply #12 on: July 12, 2011, 07:41:22 AM »

Oh sorry Julie, I forgot to say thanks for the write up Smiley