Frit-Happens !
October 29, 2020, 05:23:42 AM *
Welcome, Guest. Please login or register.

Login with username, password and session length
your ad here
News:
Where are you?? Add yourself to the NEW FHF map here  | On flickr? Join our Frit Happens group: here

VISIT THE WIKI HERE
Get FH Status updates via twitter @FritHappens

 
   Home   Help Search Calendar Login Register  
Pages: 1 [2]
  Print  
Author Topic: Themed S&T: BLUES, TURQUOISES, AQUAS, GREENS  (Read 6855 times)
0 Members and 1 Guest are viewing this topic.
SueP
Forum Member
***
Posts: 247



WWW
« Reply #15 on: September 04, 2008, 04:08:34 PM »

A few from me:

First "Think Ink" Grin



and a green goddess  Wink

Logged

SueP
Forum Member
***
Posts: 247



WWW
« Reply #16 on: September 06, 2008, 10:10:20 AM »







 Grin Grin
« Last Edit: September 06, 2008, 10:12:15 AM by SueP » Logged

turquoise
Morello Beads
Forum Member
***
Posts: 102


Beads beads beads


WWW
« Reply #17 on: September 07, 2008, 01:26:30 PM »

There is some turquoise hiding in these and light silver purple and ivory.
Very swirly my first time making these, I did have 5 one dropped on the floor bounced around the kitchen and broke!!!


A big photo, sorry.
Vicky Grin
« Last Edit: May 17, 2010, 01:28:42 PM by Billie » Logged

Zeldazog
My name's Dawn, I'm an
Administrator
*******
Posts: 1048


I'm free, to do what I want...♪♪♪


« Reply #18 on: September 16, 2008, 10:12:12 AM »

My brother and sister-in-law are both mad on squirrels, and I made a set of these for them last Christmas - I never got chance to post them before, as they didn't actually come out of the kiln until Xmas Day morning!

But I got one back to photograph recently so I can show an example at my next craft fair and show it on the website/blog.

So here it is - kiln-carving....   


And to show the reverse side     



Logged

dinah46
Forum Member
****
Posts: 358



WWW
« Reply #19 on: September 16, 2008, 01:03:45 PM »

Lovely squirrel Dawn, very effective Cheesy


Here's my contribution to the blues, I love lapis Grin
Logged

misspixie
Guest
« Reply #20 on: September 20, 2008, 04:30:49 PM »

I have a set of bumpy's... Rare for me, I'm rubbish at making sets!

Logged
turquoise
Morello Beads
Forum Member
***
Posts: 102


Beads beads beads


WWW
« Reply #21 on: October 12, 2008, 11:13:27 AM »

I had a go at etching and made these with my new bead press.


I also made these dotty ones.
Logged

Charli
Forum Member
*
Posts: 48


« Reply #22 on: May 27, 2010, 01:45:38 PM »

The first time I've got reduced glass to work! It rusn out it works much better in hot weather than cold (I work outside so the temperature does effect stuff)

This is triton


And this was triton with JetAge Studios Opal Fritt over
Logged
gülperi
Guest
« Reply #23 on: June 04, 2010, 12:01:36 PM »

some blues







Logged
madpup
Forum Member
***
Posts: 104



« Reply #24 on: June 07, 2010, 06:00:56 PM »

Its been a while, so inspired by a course i did at FO.....


« Last Edit: August 11, 2010, 05:00:15 AM by Jolene » Logged

Instead of getting married again, I'm going to find a woman I don't like and just give her a house.


www.madpup.co.uk
lampworkbyamy
New Forum Member
*
Posts: 13



WWW
« Reply #25 on: July 23, 2010, 10:51:18 PM »

I made these beads with CiM Poison Apple, Gaia, and Moretti 026 Teal.




« Last Edit: July 24, 2010, 02:58:28 AM by Jolene » Logged

lampworkbyamy
New Forum Member
*
Posts: 13



WWW
« Reply #26 on: August 11, 2010, 04:51:35 AM »


These ones I made into a necklace for my mom, because she had a dress that was in these exact colours (and, I hadn't even seen/heard about the dress when I made the beads, it was just an awesome coincidence!)




CiM Poison Apple and DH Gaia


Some CiM Leaky Pen and Light Turquoise
Logged

Jolene
Forum Member
*******
Posts: 1032



WWW
« Reply #27 on: August 11, 2010, 05:07:57 AM »


turquoise-sea-lentils--3 by kitzbitz art glass by Jolene, on Flickr
Effetre 034 light trans Turquoise


olive-geode-2 by kitzbitz art glass by Jolene, on Flickr
Geode, outer layer is CiM Olive with white enamel flecks
« Last Edit: August 11, 2010, 09:22:17 AM by Jolene » Logged

Pages: 1 [2]
  Print  
 
Jump to:  

Powered by MySQL Powered by PHP Powered by SMF 1.1.21 | SMF © 2015, Simple Machines Valid XHTML 1.0! Valid CSS!
Page created in 0.04 seconds with 20 queries.