Bead Release Problems

Started by Kay24, February 21, 2011, 09:23:03 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Sarah

I use fusion and have no problems with flame drying. But I usually let the mandrels stand for about 10 - 20 minutes before I use them and I dry them behind the flame so that they dry slowly.

If you water your release down too much just leave the lid off for a while and it will thicken again.

Sarah
xxx

★★Terri★★

Quote from: Pat from Canvey on February 22, 2011, 09:05:32 AM
For the last few months, I've started to remove the dried bead release from the mandrel after the bead is made by rubbing it through my fingers straight into the bin. I find that the beads then come off the mandrel after say only a 10 min soak in water. I clean any other release off the mandrel in water only but always dry each mandrel on paper towel.

Please be careful with dry bead release it has a lot of silica in it - which breaks up into very fine airbourne particles and will cause serious damage to your lungs when inhaled.  You should always take care if you are brushing it off when it's dry and wear a dust mask/ventilator and use ventilation, or keep it damp to prevent dust.  The dust from breaking it up when dry will stay floating in the air for hours.