Encasing! ...or lack thereof

Started by DeanWilson, February 16, 2011, 01:07:50 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

DeanWilson

Had a go with some of these methods and actually had a moderate degree of success!! :P Shocking!! :P ;D

Just had an idea though....Could you use clear glass frit to encase your beads? Very finely ground to give a really even coating? And because it's glass obviously it would all blend in evenly anyway! Has anyone tried this before?

Dean ;D x

MadelineBunyan

in glass casting, the bigger the chunks you use, the better clarity you get, and when you cast in frit, you get cloudy. I guess this would be the same with a bead.

you could try it, but you'll need to wash your frit very thoroughly, every speck of dust dirt grease, etc will probably result in scum,or some other unpleasantness. perhaps the results will be interesting, may take you down an interesting arty path, but sadly I dont think it will result in beautifully clear encasing.

encasing is a skill worth persevering with!