Frit-Happens !
January 19, 2021, 07:58:53 AM *
Welcome, Guest. Please login or register.

Login with username, password and session length
your ad here
News:
Where are you?? Add yourself to the NEW FHF map here  | On flickr? Join our Frit Happens group: here

VISIT THE WIKI HERE
Get FH Status updates via twitter @FritHappens

 
   Home   Help Search Calendar Login Register  
Pages: [1]
  Print  
Author Topic: Anyone here work with bullseye?  (Read 2876 times)
0 Members and 1 Guest are viewing this topic.
bubblefizz
Guest
« on: June 13, 2007, 03:41:55 AM »

If so what do you think of it?
whats it like to work with?
and most of all where the heck do you buy it? lol Grin i only know of warmglass!
Logged
MyPrecious
Forum Member
****
Posts: 277



WWW
« Reply #1 on: June 13, 2007, 04:28:44 AM »

I got mine from  www.howacoglass.com
Logged

Sulis (Hazel)
Forum Member
***
Posts: 206



« Reply #2 on: June 13, 2007, 06:08:59 AM »

I can supply Bullseye if you're interested. Just putting together a list of what I can get hold of - prices are pretty reasonable. Is there anything in particular that you are looking for?
Logged

Hazel x
bubblefizz
Guest
« Reply #3 on: June 13, 2007, 07:36:12 AM »

Hya Hazel, well im not looking for anything inparticular yet, i just want to try it out Roll Eyes

but i love pinks and purples lilacs etc... Grin Grin
Logged
Billie
Rompin', stompin'
Forum Member
*****
Posts: 602



WWW
« Reply #4 on: June 13, 2007, 09:32:05 AM »

I admire you Angie.  You love experimenting with new stuff  Grin
Logged

Sulis (Hazel)
Forum Member
***
Posts: 206



« Reply #5 on: June 13, 2007, 09:52:03 AM »

How about a trial bundle of pinks/purples and a couple of complimentary colours? I'm not a proper supplier yet (just thinking about setting up), so would need to work out a price for you, then postage would be at cost anyway so shouldn't be expensive. How much are you looking to spend roughly? If you want to pay via Paypal, I could even post out to you straight away so you could be playing with Bullseye by the weekend  Wink It's great fun! An added bonus is that you can use rods but also sheet glass, dichro stringers and dichro frit, ordinary frits, powders and all sorts of compatible inclusions - the possibilities are very interesting to say the least  Grin   My supplier does all those too!

PM me with your request and I'll see what I can get hold of for you. Any excuse for a lunchtime trip to drool over glass Wink
Logged

Hazel x
fosterfire
Guest
« Reply #6 on: June 17, 2007, 04:10:46 PM »

Just wait until you try transparent neo-lavender over their red or over their pink!!  It's absolutely hot, hot hot!!
Logged
Sulis (Hazel)
Forum Member
***
Posts: 206



« Reply #7 on: June 18, 2007, 01:22:55 PM »

Oooh - I think I picked up some of that  Wink Looks yummy to me!
Logged

Hazel x
petrahergarden
New Forum Member
*
Posts: 14


« Reply #8 on: March 27, 2020, 09:40:08 AM »

I use sometimes Bullseye because the lovely colours, and for clear i use Schott 90 rods, works very well
Logged
Dietmar
Forum Member
*
Posts: 37


« Reply #9 on: March 27, 2020, 06:06:56 PM »

Yep, Bullseye has a lot of different colors. I love their old Ringmottled styles, because I like to play with the opacifier. They have two very interesting shades of aventurin green and sometimes aventurin blue. All these metallic colors are very usefull partners in color mixing.

For a nice sparcling spring green mix (not fully complete) opaque yellow and some dark aventurin green.

Try also the two colored streaky styles for base beads and spacers. They make a nice variety of shades and striations for spacers. If you add most of the glass by dotting instead of winding in layers, the beads get a total different patern.

The SCHOTT AR-glass has a much higher viscosity than BULLSEYE. The viscosity of Uroboros COE90 glass is in between AR and Bullseye. Try to use it to your advantage.
« Last Edit: March 30, 2020, 06:16:06 AM by Dietmar » Logged
Moira HFG
Half Full Glass
Forum Member
****
Posts: 407


Ever the optimist


« Reply #10 on: March 29, 2020, 01:59:22 PM »

I love the way threads are reappearing!

I sometimes work with Bullseye rods, it’s quite firm and seems to hold the heat well, which is excellent for sculptural work.

You can get the rods - also frit - from Warm Glass (UK), or from Glass Studio Supplies. If you have sheets of Bullseye you can slice them and use that, but rods are nicer to work with.

Here's something I made recently. The base bead is in Bullseye Seaweed - it's a lovely streaky green with aventurine sparkles!

Lily bead

Lily bead back
« Last Edit: March 29, 2020, 03:27:37 PM by Moira HFG » Logged

beadysam
BeadySamGlass.Com
Forum Member
*****
Posts: 635


I type before I think....


WWW
« Reply #11 on: March 30, 2020, 02:27:10 AM »

I have never tried Bullseye, but some of the colours are very lickable!   I have always been impressed their website and educational content too.  I must get some when I have some spare dosh,  and Satake glass is another one on my must try list! 


Moira that flower is a stunner!!!
Logged

Margram
Temperature's rising
Forum Member
*****
Posts: 690


Glass in pocket


« Reply #12 on: April 05, 2020, 12:48:23 PM »

Trudi (glitteringprize) uses bullseye for the gorgeous pinks, I seem to recall.