Is there anything I can do??

Started by Pam, January 17, 2011, 05:57:06 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Kalorlo

A punty is basically a handle that you remove when you're finished. You can use stainless steel punties as well as glass, so a mandrel *could* be a punty  :D

james M knox

Quote from: Weston_glass_man on November 25, 2012, 10:34:34 PM
Feeling thick here but if I don't ask then I wont know... "covering face as he types" what is a punty is it a mandrel or something diff. Sorry stupidity is my gift!!!! lol :)

Just remember, the only truly stupid question is the one that you did not ask.....

James

Weston_glass_man

I say that to trainees all the time.. lol thx