★★Terri★★

I was working on the encasing skills(lol) yesterday and noticed that I was getting some 'thermal cracking' with silver glass.  This is the first time I've got silver glass to do something for me - yay - and then it cracks.  Getting to the point - I think I was letting the glass on the mandrel get too cold while melting the clear and as soon as I put the hot encasing glass on I felt and heard the bead crack on the mandrel. :'(  I suppose it's just part of the process of learning how near to keep the bead to keep it hot enough without getting in back in the flame and losing the reduction.

Gordon

I'm having a little trouble keeping the reduction on "Electra" I think I'm letting it get too hot when I encase it but it's early days I'm sure we'll 'crack'  ;) it soon enough

G