Frit-Happens !
January 23, 2021, 03:39:26 PM *
Welcome, Guest. Please login or register.

Login with username, password and session length
your ad here
News:
Where are you?? Add yourself to the NEW FHF map here  | On flickr? Join our Frit Happens group: here

VISIT THE WIKI HERE
Get FH Status updates via twitter @FritHappens

 
   Home   Help Search Calendar Login Register  
Pages: [1]
  Print  
Author Topic: Silver Black v Gunmetal  (Read 5087 times)
0 Members and 1 Guest are viewing this topic.
Lush!
Julie
Forum Member
*******
Posts: 1145


Queen of Buttons :0)


WWW
« on: February 21, 2011, 04:10:39 AM »

I did a quick comparison between Effetre Silver Black and CIM Gunmetal.

The Silver Black does fizz and boil when you're working it whereas the Gunmetal is much better behaved.

The Silver Black kind of strikes from shiny to satin and back to shiny as you heat and cool, the Gunmetal pretty much stays the same whilst working it.

Adjusting the flame chemistry doesn't make much difference to the Silver Black; bathing the Gunmetal in an oxygen-rich flame at the end brings out the silver sheen.

Really working and 'abusing' the Silver Black can produce fabulous peacock colours - I couldn't get the same effect from Gunmetal.

The two hearts on the left are Silver Black, the one on the right is Gunmetal - they all look very similar, I suppose the Gunmetal is shinier.  But there's a marked difference in the spacers (SB on left, GM on right)


Metallic by LushLampwork, on Flickr
Logged

Pages: [1]
  Print  
 
Jump to:  

Powered by MySQL Powered by PHP Powered by SMF 1.1.21 | SMF © 2015, Simple Machines Valid XHTML 1.0! Valid CSS!
Page created in 0.028 seconds with 20 queries.