Author Topic: champagne bubbles, how to..  (Read 4576 times)
0 Members and 1 Guest are viewing this topic.
madpup
Forum Member
***
Posts: 104



« on: July 13, 2010, 10:06:03 AM »

Thought i'll have a bash at this, there are two going up
but this one is there now...enjoy.
http://www.youtube.com/watch?v=Xj12N9IMF0Q
Logged

Instead of getting married again, I'm going to find a woman I don't like and just give her a house.


www.madpup.co.uk
madpup
Forum Member
***
Posts: 104



« Reply #1 on: July 13, 2010, 10:34:19 AM »

And this is the second,
http://www.youtube.com/watch?v=llXKj1IfvLo
 Wink
Logged

Instead of getting married again, I'm going to find a woman I don't like and just give her a house.


www.madpup.co.uk
beadammed
Forum Member
***
Posts: 106



WWW
« Reply #2 on: July 13, 2010, 05:48:21 PM »

Thanks for that.  I wondered how it was done
Logged

★★Terri★★
Forum Member
***
Posts: 186


« Reply #3 on: July 13, 2010, 05:52:31 PM »

I have been playing with champange bubbles for a couple of weeks - and found them surprisingly easy to achieve (or perhaps beginners luck).  Only trouble is loads of the beads I have used them in have cracked on the mandrel.  But then I have been putting murrini in and pressing them as well. 

Terri
Logged
madpup
Forum Member
***
Posts: 104



« Reply #4 on: July 13, 2010, 09:06:48 PM »

Terri i have not had a problem with cracking (touch wood) are you using soft glass (104)
or it might be the clear, i have heard of some peps having trouble with certain clears?
thanks beadammed, i try to please lol.
Logged

Instead of getting married again, I'm going to find a woman I don't like and just give her a house.


www.madpup.co.uk
★★Terri★★
Forum Member
***
Posts: 186


« Reply #5 on: July 14, 2010, 04:06:40 AM »

Yes I am using Eff crystal clear.  Some crack - some don't.  The crack always follows the line of the hole along the mandrel and is on both sides of the bead.  I am sure it is something I am doing wrong - but when I use other glasses to make lentils they don't crack Huh
Logged