Frit-Happens !
September 18, 2020, 03:55:47 PM *
Welcome, Guest. Please login or register.

Login with username, password and session length
your ad here
News:
Where are you?? Add yourself to the NEW FHF map here  | On flickr? Join our Frit Happens group: here

VISIT THE WIKI HERE
Get FH Status updates via twitter @FritHappens

 
   Home   Help Search Calendar Login Register  
Pages: [1]
  Print  
Author Topic: if i wanted to do this what wire would i need?  (Read 3097 times)
0 Members and 1 Guest are viewing this topic.
flowerjasper
Forum Member
****
Posts: 470


Acorns!


WWW
« on: June 07, 2010, 05:16:24 PM »

I would love to have a go at spirals like this, i have brought some 0.8 and 1mm silver plated wire to practice with, (hobby craft has just opened up near here, so i brought a tiny hammer too  Wink)
should it be  round wire ?
i also have the encyclopedia of wire jewellery techniques by sara withers,
first attempts on wednesday when the boys go to their dads  Wink
sandy x
Logged

mizgeorge
Administrator
*******
Posts: 795


Or should that be missus?


WWW
« Reply #1 on: June 07, 2010, 05:24:47 PM »

Is there a picture or link Sandy?
Logged

flowerjasper
Forum Member
****
Posts: 470


Acorns!


WWW
« Reply #2 on: June 07, 2010, 05:49:24 PM »

sorry  Embarrassed
me being blonde again!

sandy
« Last Edit: June 07, 2010, 05:51:30 PM by flowerjasper » Logged

mizgeorge
Administrator
*******
Posts: 795


Or should that be missus?


WWW
« Reply #3 on: June 07, 2010, 06:17:44 PM »

I'd start with 1.3mm wire for something like this - and you might want to try copper (which is likely to be 1.25 if you go to wires.co.uk) rather than plated - the plating will crack and split if you forge it. Round wire is perfect - you just forge the edges which are going to be subject to most stress to stop them from unbending.
Logged

flowerjasper
Forum Member
****
Posts: 470


Acorns!


WWW
« Reply #4 on: June 08, 2010, 02:18:14 AM »

will get some copper wire george,
i did think about the plating....
for ear wires whats the best thickness?
you are going to get fd up with my questions very soon  Cheesy
sandy
Logged

ScarletLeonard
or Scarlett, or Scarlette
Forum Member
****
Posts: 424



WWW
« Reply #5 on: June 08, 2010, 02:39:19 AM »

Copper is certainly a better option it's so much easier to practice with and easier to see the details of the end result too.
To do something like that I would hammer the areas I want flat with a flat brass head then go over the whole wire with a nylon head to harden all the parts rather than just the stress areas.

Earwires apparently 0.71 is the optimal thickness most people will use 0.8mm since it is a little easier to buy though I do prefer 0.6 I find it doesn't pull the ear holes as much but it isn't very forgiving if it isn't fully hammer hardened.

Scarlet xx
Logged

flowerjasper
Forum Member
****
Posts: 470


Acorns!


WWW
« Reply #6 on: June 08, 2010, 05:38:20 PM »

a new craft for me so lots to learn  Roll Eyes
thanks for the earwire info scarlet  Wink
am on wires uk at the moment i hope i get the right stuff, a selection of copper wire  would be the best,
sandy x
Logged

mizgeorge
Administrator
*******
Posts: 795


Or should that be missus?


WWW
« Reply #7 on: June 08, 2010, 06:03:13 PM »

I'm not keen on 0.7 for earwires - it's tough to get it to hold good shape without overforging, which can leave sharp edges, so I tend to use 0.8, and usually fully hard at that. I have a slight preference for Argentium over Sterling.
Logged

MadelineBunyan
*insert custom title here*
Forum Member
*****
Posts: 511


Devon Glass Addict


WWW
« Reply #8 on: June 08, 2010, 06:12:55 PM »

does no one else draw down their wire for earwires? gets it to the thickness you want and then is perfect hardness!I do about 0.7 (or the imperial equivalent...my drawplates are OLD!) because its what I personally like. I find thinner ones can look/feel as though they're cutting your earlobe like cheesewire!

(I do have to remember when drawing down wire to open the door behind where the vice is or I smack my elbow into it!  Roll Eyes )

you can get drawplates cheap on ebay, just be sure to check the sizes. theyre not that good quality, but they work fine.


oh, and a tip...shiny polished hammer = less work to make the thing you are hitting with it nice and shiny!

hmm, do I want to spend my time polishing one hammer, or every item I ever hit with it?

Logged

ScarletLeonard
or Scarlett, or Scarlette
Forum Member
****
Posts: 424



WWW
« Reply #9 on: June 09, 2010, 02:46:42 AM »

I don't have the space to do my own, I'm already close to bashing my elbow every time I pick up a glass rod. Sad

On wires they do have the selection packs which are great because you will get 0.4mm all the way up to 1.25mm
Actually I also have a 3 meter length of 1.25 you can have if you want some extra. (You may have gathered I'm not keen on super chunky.)

Scarlet xx
Logged

fionaess
Global Dominator
Forum Member
*****
Posts: 567



WWW
« Reply #10 on: June 11, 2010, 12:27:58 PM »

I use .8 hard round for earwires as well - I find it works perfectly and no wiggle or bend  Grin
Logged



If it's got a hole, it's a bead !
jammie
Do what you can, with what you have, where you are
Forum Member
******
Posts: 754



WWW
« Reply #11 on: June 20, 2010, 04:15:35 AM »

I had a look on wires.co.uk and can only find largish quantities of wire, I want some square for making a fibula for myself and some 0.8 for earwires (as you have said is best here) anwhere else good I can buy this in smaller amounts please. Havent much cash at the mo and just wanted to try them out. (I have some copper to start with already)
Logged

mizgeorge
Administrator
*******
Posts: 795


Or should that be missus?


WWW
« Reply #12 on: June 20, 2010, 07:13:49 AM »

I think wires usually sell just a metre of wire. Otherwise, palmer metals are good for small quantities.
Logged

jammie
Do what you can, with what you have, where you are
Forum Member
******
Posts: 754



WWW
« Reply #13 on: June 20, 2010, 11:45:02 AM »

I could only find 10m of sterling in the 0.8 at about 37 quid ish,in wires.co   the fine silver is in metres but fine silver would be too soft for the earwires wouldn't it.
Had a look on palmers and they seen to do by the metre.