Author Topic: 6mm SLUMPING firing schedule (ARTISTA)  (Read 3870 times)
0 Members and 1 Guest are viewing this topic.
handmadeheaven.biz
Guest
« on: January 06, 2007, 10:59:50 AM »

SLUMPING 6mm firing schedule ARTISTA

1. 175C/hr to 540C   0.10

2. AFAP or 9999C/hr to 700C   0.00

3. 100C/hr to 790C   0.00

4. AFAP or 9999C/hr to 560C   1.00

5. 66C/hr to 443C   0.00

6. 125C/hr to 393C   0.00

7. AFAP or 9999C/hr to 25C   0.00
Logged