Main Menu

Themed S&T : Boro

Started by Chameleon, May 18, 2008, 11:49:55 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Chameleon

Ok I know there are a few people dabbling in the dark side now, I have just started and would love to see what everyone else is doing (including what glass it is if you know) so marbles, beads, sculptural anything & everything boro .... please  ;D

to start us off -


and a couple of silver cores

come on what does everyone else have ....  ;D ;D

edited 3/6/10 added new pics as pics had vanished

garishglobes

It would be good to see this thread a bit more active again, I can't think where else to put this and I do want to show and tell, so - this is a Caramelo Light hand with red vortex using GA Cherrywood dichro stringer as well as a few anonymous ones (cloud, unobtanium and ??)