Can anyone help me I,ve just bought some bullseye glass and was wondering if it would be ok to use beadie sams frit with it .the glass is coe90 and i noticed the frit is 89 to 96 .
xxcatxx

Josephine

Should be ok. Most of us use it with 104 coe glass so  the difference is actually less with the bullseye.

*rowanberry*

I use bullseye now and again and the frits were no problem.
Claire

catriona

Thanks girls will now give it a go .