Started by firedinglass, November 11, 2015, 10:36:53 AM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

firedinglass

My tumbler,shot,has,gone,rusty after,I,left it too dry, I now,remember that I should leave it in a soapy solution. I have read various tips on cleaning it,and,the tumbler ,  from TSP ( never tried) , barrelbrite ( think mine must,have lost it's strength) Eco washing crystal, Fairy liquid,and  Flat Coke!
  Does anybody  have experience or comments  on these!


www.facebook.com/firedinglass
http://www.etsy.com/shop/firedinglass
Lisa

mizgeorge

The problem with using regular shot (rather than stainless, which is more expensive) is that unless it's completely dry it will rust.

In honesty, it's probably best to just buy a new bag.

firedinglass

I have found some other shot in the depths of my workshop that is OK.
But I would like to ask you how it is best to store it between use , as I only use it occasionally?
Also would you recommend using flat Coke to clean the barrel of a second hand Lortone I have managed to find?
Not sure which medium it was used for, rocks or jewellery. It was described as a gem sparkler.
Thank you so much  George for all your invaluable advice!


www.facebook.com/firedinglass
http://www.etsy.com/shop/firedinglass
Lisa

mizgeorge

I just pop my barrels (just the rubber components) on the top rack of my dishwasher. Seems to work fine!


JanieD

Quote from: mizgeorge on November 11, 2015, 08:06:30 PM
I just pop my barrels (just the rubber components) on the top rack of my dishwasher. Seems to work fine!



Nice tip George, definitely pinch that one! :)


Jane