Paragon SC2 questions

Started by GlassOcean, November 11, 2007, 08:28:05 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

GlassOcean

Hi you lovely clever and very helpful lot!!!  ;)

Do any of you know the answers to a couple of questions?

1. How long from closing the kiln door and running the batch anneal for SC2 detailed above can I open the door and take my beads out?

2.Does anyone know how much it costs money-wise to run a batch annealing cycle in the SC2?

Ta loves,
KJ.

glassworks

the beads can come out when they have cooled enough to carry - anything under 50 degrees C is about as long as griet has ever been able to last!!

;D ;D

the annealing cycle costs pennies - the kilns are efficient and very well insulated..

;)

GlassOcean

Lovely, thanks Q.  Griet is a girl after my own heart, I have to physically stop myself opening the door too soon!!!

I am sure this obsession must wear off!!!!   ;)