Bigger work without a kiln?

Started by sparrow, October 22, 2007, 09:26:10 AM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

sparrow

Hi, the off-the-mandril calla lily tutorial Jolene linked to looks soooo lush, but I noticed that, anytime the work is gigger or complex, it says 'pop straight in the kiln' (which for me means 'pop straight under the fire blanket') - should I steer clear of this kind of stuff until I can afford a kiln? I think I'd be heartbroken if I tried a batch of lilies and they came back cracked from annealing :( :(
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

Marijane

I have been practicing off mandrel leaves while I wait for the kiln to warm up, and none have broken.  Just make sure the overall thickness does not vary too much.

Mari