flame n fuse

Hi, I was wondering what experiences others have with interesting reactions between bullseye glasses. I have the info sheets, but most of the reactions I get are of the 'thin dark line' variety, apart from interesting reddish reductions with teal and the nice reactions vanilla and nougat have with blues. Does anyone get anything else? I am jealous of the reactions I see with some of the other glasses on frit happens.