I got a square graphite mandrel this moring (YAY!) and was wondering if I put bead release on it? I'm guessing yes, but just needed to double check....
Thanks xxx

SilverGems89

hmmmm my guess would be yes Helen because the glass will stick to the bead release but not to the graphite...although whether the bead release will stick to the graphite is another question!  ;D

helenfc

 :D this is true! Thanks, I guess there is nothing to lose eh? x

JKC

Hi Helen, they sell some here  www.inspirationtoolworks.com and have a tutorial, they are slightly different ones, but the way of using them should be the same.  Janet