Started by Pam, January 10, 2007, 04:38:12 PM

Previous topic - Next topic

0 Members and 4 Guests are viewing this topic.

Pam

What do you think of this.
Real hole, very smooth and quite funky. Haven't got a clue how they got there but really like them.
I have a couple more fusing to do on this before it is complete but just wanted to share my confusion over the holes.

handmadeheaven.biz

lovely colours Pam ;D i think the holes are probably air bubbles. how thick was your glass? i expect they were air bubbles which got bigger, then burst leaving a small hole and as the glass has settled it has drawn up the glass around the burst bubbles, leaving holes. that's what i reckon anyway!!

doubleglazed

i think the holes are cool would make a great beadwork progect

*rowanberry*

i really like that!!!!!!!
Claire

xtweeksx

Ooooooooo I really really like that!!

Can you do it again on purpose? hehe  :)

Soozintheshed

Yeah I like it lots too, I want to make one  :)
Sooz     '(0,0)'



www.thebeadshed.co.uk
http://stores.ebay.co.uk/The-Bead-Shed

Soozintheshed

I made these last night, any tips on avoiding the bubbles  (although I do quite like the bubbly look)
Sooz     '(0,0)'



www.thebeadshed.co.uk
http://stores.ebay.co.uk/The-Bead-Shed

handmadeheaven.biz

one way is to put the small pieces on top, that way you won't trap any air. I think they look nice tho!

xtweeksx


Carol

I really like them with the bubbles Sooz!
Carol

♥♥Tan♥♥

I am so jealous you are all having a go and producing really great stuff, I must pull my finger out

How big is that piece Pam?

Pam