Main Menu

Fused Tile Tutorial

Started by Lildee, December 29, 2009, 11:06:45 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Lildee

Hi, this is a Fusing Tutorial for very easy to do (and cheap to make) pretty glass tiles. Would love links too!
HAPPY NEW YEAR TO ALL xxx Lildee




http://www.users.globalnet.co.uk/~dee/Tutorials.htm