Kiln temperatures

Started by Edi (Edith), September 03, 2009, 01:40:14 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Edi (Edith)

I have turned on my new kiln today Paragon SC2. and I am following the instructions for the Ramp Hold practice programme and it is in F and the kiln was set in C so OH has changed it to F is that what most people use. I am getting more and more confused.
Edi
Nana to 5 beautiful girls

mizgeorge

Hi Edi,
I think most of us here use C. There are some excellent schedules posted on the forum, and I think all of them are in C. I used to use Helen P's schedule for my SC2, and had no problems with it at all.

Trudi

It's not really a problem which you use, but if you're asking questions or comparing what most people would do on here then °C is more useful for you!