Main Menu

Tarnish-proof Copper Wire

Started by Shirley, February 17, 2013, 09:31:14 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Shirley

Tomorrow I'm off into town to buy some copper wire from an ironmongers. I've rung them up and they have told me the wire is anti-tarnish. The question is, will I be able to do anything to it to get an aged finish? Not sure I want the bright finish all the time.
Val Cox Frit - Thai and Bali Silver 

Lakelady

I have tried to tarnish anti-tarnish copper wire and it doesn't work  :D
Turner Rowe Glass Art

Shirley

Ok, shiny it is, then :D It's mainly for practising before I buy silver
Val Cox Frit - Thai and Bali Silver 

mizgeorge

You can remove the coating by burning it off, or by running the wire fairly vigorously through a sheet of micromesh or wet an dry paper. If it's just for shaping practice, though, it's probably just as easy to leave it as is!