Main Menu

Spinning top tutorial

Started by Steampunkglass, February 18, 2010, 11:20:41 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Steampunkglass

Found this rather fun spinning top tutorial. It's boro, but says it could be done with soft glass if you keep it warm.

http://www.everafterartistry.com/freetoptutorial.htm

Tracy


SuefromYorkshire

Really like these  8), never have thought to make a spinning top from glass,
thank you Glen! ;D

Chameleon

Ooo thanks Glenn, I have been meaning to look for one for ages  ;D ;D

Studio Girl

when I click on it says video unavailable

garishglobes

There is a pdf file though, with lots of piccies :)
She notes at the end that a graphite knob mould is available.... interesting... ;D