Has anyone ever etched any of the mystic colours - and, if so, how did they turn out?
Has anyone etched multicolour - what happens?
Has anyone etched frit beads on a silver foil base - what happens?
Just before I do......
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

princess pink

Lol! So many questions!! I can only help with multicolour cuz I know Kate (of the sublime nature) etched some mc discs. Will have to find the thread though!

Lush!

Mystics etch fab - I etch the blue, green and grey regularly  ;)


www.lushlampwork.etsy.com

hollergrafik

MC looks fab eteched, did a set of 5 button beads.

Kaz

Thanks folks - I have some lovely mystic beads that have de-vited slightly in a couple of places so I think etching may work out well.
Got to try the MCD too!
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

hollergrafik

kaz if the mystic gets the devit around the mandrel give it a nice bathe in mid to top flame until it has a good glow, the devit goes.

Kaz

Thanks Kay - I'll try that next time!
In the meantime, they etched nicely

Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Lush!

Oh yes, indeed they did!  I think the Mystics should be called Velvets instead actually  ;D


www.lushlampwork.etsy.com

♥♥Tan♥♥

Gorgeousness Kaz, aren't you glad you asked though ;)

SMHBuss

I etched some mc and didnt like it.  Will try and post some pics in the next few days.

Amber

I just etched some mcd and it looks great!  :D

SMHBuss

Ooops.  I forgot.  The ones I etched I sold.  So they must not be that bad!!  :)