MONTHLY THEME CHALLENGE - September

Started by Krysia@No98, September 02, 2013, 08:56:22 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Krysia@No98


What a shame!!  Other wise she's great!
-* -  Courage is going from failure to failure with out loosing enthusiasm -*-

Jane C ♫

That chicken is awesome - great character! Good luck fixing her (or with the next one)!
Hand Painted Silk and Fused Glass Artist.
Lampwork Beginner!
Website

Glassy Lou

#17
Here's my little contribution... a little portly chap :)


Penguin by GlassyLou, on Flickr

Pat from Canvey


Glassy Lou


Skyblue



A little Wren. This is I think my third attempt at making a birdy so be kind please .:)

Trudi

Great start .... There were a few more made yesterday at Angie's open studio!

Jane C ♫

Hi Skyblue. Great body shape and I love the colour - very subtle.
Hand Painted Silk and Fused Glass Artist.
Lampwork Beginner!
Website

Skyblue


katie78

I am still a proper newbie to this lampwork lark so have decided to keep it simple and consulted the 6 year old me in how best to make a bird bead and we both decided that a 'M' shaped bird with a sun and sunbeams was the only way forward  ;D


I hope you like it  :D




One of the sunbeams broke off when I was taking him off the mandrel, poop!!

Yeske

It is a very cute bead :) Very sunny, nice idea!

I was thinking about making something with M-shaped birds as well, since I haven't done any sculpting yet.. But I haven't had the time :P

jeannette



flowerjasper

lovely birdies so far, really great to see newbie work  ;)
a tiny bird from me, this one comes with a free bubble !

copper by Flowerjasper2, on Flickr
sandy

katie78

Thank you ladies  :)

He was a lot of fun to make and I must admit I was giggling like a little kid making him  ;D