Kaiser Lee Board

Started by fleurbrawl, August 02, 2009, 05:42:25 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

fleurbrawl

Is anyone else using this stuff for slumping?
Can you use kiln wash on it or do you have to stick with thinfire paper?
Kays' OH :)


2B or not 2B, that is the pencil.

Nina A

I've used kaiser Lee, and I used Kiln wash for the first three of four firings,   I then use a bit of thinfire for the next couple just in case.

fleurbrawl

Thanks,
the shape I've carved lends itself better to wash than thinfire.
I'll give it a few coats and see what happens.
Kays' OH :)


2B or not 2B, that is the pencil.

Warm Glass UK

It can also be fired without kiln wash!

Pippa

fleurbrawl

Kays' OH :)


2B or not 2B, that is the pencil.

Zeldazog

I have used without kilnwash, and it doesn't stick to the glass.  However, the glass did pick up the texture of the Kaiser Lee board (which was quite nice!)

I *think* you can sand paper it (perhaps Pippa can confirm this) - but USE A DUST MASK!


fleurbrawl

I did rub one of the offcuts with a bit of sandpaper and that did work.
I've used the back of a blade to smooth down the areas that were cut. Quite like the texture left on the top.
But I know what you mean about the dust... and the glass splinters, great fun picking them out of my fingers.
Kays' OH :)


2B or not 2B, that is the pencil.

Warm Glass UK

Yes, it can be sanded - we use fine grade paper in the studio here to get a really smooth finish where desired. Definitely, as when you are using any fusing products which contain particles such as frits, powders etc, we always wear a Dust Mask and would recommend others to do likewise. At least because this stuff is prefired, it doesn't give off unpleasant fumes on firing!  :) Pippa

fleurbrawl

I've tried a firing without kilnwash/paper now.
Worked quite well and did indeed pick up every bit of the texture. It also took a while to get the KLB bits out of the glass :)

I'm going to try again later with the same mold kilnwashed. It's been drying for a couple of days now.
Kays' OH :)


2B or not 2B, that is the pencil.