Ok here is how I do that kinda stringer..............

1. cut some silver leaf the length of the square by about 1" place on your non flamable work surface/marver
2. take one commercially pulled ivory stringer
3. If your posh dip your finger in water, if your like me a good bit of slobber works fine  Wink wet the first 4" (or how ever long your piece of silver leaf is) of the stringer.
4. Roll your stringer over the silver so it wraps around your stringer, the wet will make it cling like a magnet.
5. flash through the flame quickly and gently to burnish the silver to the stringer.
6. apply to your bead by laying it on and let it melt in....voila!

Lorna XX


Title: Re: Silvered Ivory Stringer by Pixiewillow
Post by: sparrow on November 28, 2008, 07:47:55 AM
Is it on the wiki?  ;D


Title: Re: Silvered Ivory Stringer by Pixiewillow
Post by: Jolene on November 28, 2008, 09:08:16 AM
I have not transferred it to the Wiki :)