Tutorials in here.. => Lampworking => Tips and tricks => Topic started by: beadysam on January 13, 2007, 04:31:44 PM
Title:
Sexy Blue Bead tute
Post by:
beadysam
on
January 13, 2007, 04:31:44 PM
http://www.lampworketc.com/forums/showthread.php?t=235
Title:
Re: Sexy Blue Bead tute
Post by:
♥♥Tan♥♥
on
January 13, 2007, 05:04:49 PM
I really like this enough to have a go but what is threaded stringer
Title:
Re: Sexy Blue Bead tute
Post by:
littlegiggles
on
January 13, 2007, 05:12:03 PM
very fine stinger a bit like cotton thread
This was my attempt at these