Frit-Happens !

Show & Tell => Show and Tell => Glass colour references => Topic started by: Tracy on July 01, 2009, 11:54:47 PM

Title: Re: Gaffer Chalcedony
Post by: Tracy on July 01, 2009, 11:54:47 PM
My first go.....considering it was five thirty this morning when I played, I am  quite chuffed!
Coarse frit pulled into stringer over eff light ivory opps  ::)

(http://i707.photobucket.com/albums/ww72/ace_balloonz/Silver%20Glass/th_IMG_2383.jpg) (http://s707.photobucket.com/albums/ww72/ace_balloonz/Silver%20Glass/?action=view&current=IMG_2383.jpg) clickable!!
Title: Re: Gaffer Chalcedony
Post by: Veebee on July 07, 2009, 08:14:35 AM
Quote from: flowerjasper on July 07, 2009, 12:10:51 AM
i cant get any pretty colours ;-(
i am ok with raku  but this one.... i have tried heating, got brown, tried striking, got brown, tried not heating, got brown !!
different bases too, have followed marys advice, but ..still brown  ::)
anyone got any tips??
s x

Same here! However, I heated the snot out of this one, did the gravity swirl thing then marvered to strike, and I got colour!
(**click on the image for a closer view**)

(http://i630.photobucket.com/albums/uu26/veebeads/th_gaffer.jpg) (http://s630.photobucket.com/albums/uu26/veebeads/?action=view&current=gaffer.jpg)

Try working it for a bit longer maybe?

I used CiM Khaki as a base.
Title: Re: Gaffer Chalcedony
Post by: Trudi on July 07, 2009, 08:14:57 AM
not the best picture - but I got this

(http://i39.photobucket.com/albums/e160/shine-on2/Beads/0507016.jpg)

I've also got one on black and one on white - but I need to take pics.

Sandy all I can say is what Mary said - sorry ......
Title: Re: Gaffer Chalcedony
Post by: sparrow on July 07, 2009, 10:13:09 AM
Right, I think I was overly polite......was the restriction one per size per person?? Or one per person, full stop? I went for the latter. If anybody ever makes jokes about Germans and towels or anything else, please remember this moment, lol!!

Anyways, you've seen him elsewhere, but he's Chalcedony on black, Size one:

(http://farm3.static.flickr.com/2453/3688040760_b18afe3d69_m.jpg)

:)
Title: Re: Gaffer Chalcedony
Post by: Diane on July 07, 2009, 02:13:29 PM
Here's a shell set I've made using System96 (had it in for ages and only just using it ;D) glass and a mixture of No1 and No2 Chalcedony frits.:
(http://farm4.static.flickr.com/3600/3697192757_216a61923b.jpg)

Diane x
Title: Re: Gaffer Chalcedony
Post by: dinah46 on August 02, 2009, 08:55:35 PM
This is chalcedony stringer over silver foil, I'm beginning to really like this frit :D

(http://farm3.static.flickr.com/2468/3772160431_bb0a6dee9a_m.jpg)

these are a mixture of small and chunkier frit
(http://farm4.static.flickr.com/3449/3772964576_a39b33bf20_m.jpg) (http://farm4.static.flickr.com/3560/3772966098_ec556e5b0f_m.jpg) (http://farm3.static.flickr.com/2433/3772152845_4fa67a266c.jpg)

Title: Re: Gaffer Chalcedony
Post by: *rowanberry* on August 14, 2009, 07:41:09 PM
Wowzers Sam, they are fab!

Here's what I did with some stringers pulled from frit (cant wait to get hold of the cane!):

(http://farm4.static.flickr.com/3563/3795515962_48d364ec3f_m.jpg)(http://farm4.static.flickr.com/3459/3794694949_bea9aa8a87_m.jpg)
(http://farm4.static.flickr.com/3567/3794695147_d1a8f12d0c_m.jpg)

I found that chalcedony sometimes puts a dusky grey on ivory near where you put it. I liked it though as it made it look "old".
Title: Re: Gaffer Chalcedony
Post by: turnedlight on August 18, 2009, 03:20:28 PM
I got them out of the kiln, and I am chuffed with the results but they are a pig to photograph!
Here's the first, I heated and cooled several times, then I raked, and heated and cooled very gradually..
          (http://farm4.static.flickr.com/3433/3833851896_58fc46b0f5.jpg) (http://www.flickr.com/photos/53211004@N00/3833851896/)
And here's the second
          (http://farm4.static.flickr.com/3549/3833851888_5f135fbd58.jpg) (http://www.flickr.com/photos/53211004@N00/3833851888/in/photostream/)

Love this glass! :)
Title: Re: Gaffer Chalcedony
Post by: Trudi on September 02, 2009, 12:53:43 PM
Here's a few from me - just had a quick play:

(http://i39.photobucket.com/albums/e160/shine-on2/Beads/caravanbeadsaug09073.jpg)

I'm really pleased with the colours - but not sure about the heart. The colours are great, but it's just so obvious where I had to add more glass ........ and doesn't blend in!