Fusing and Stained Glass Tips and FAQ's => Kiln Questions => Topic started by: flame n fuse on September 12, 2015, 04:55:30 AM



Title: summary of kiln programmes for Bullseye Glass
Post by: flame n fuse on September 12, 2015, 04:55:30 AM
   
I've just found this on the warmglass website   http://www.warm-glass.co.uk/kiln-schedules-cms-74.html   
It's a useful summary and they give test results for different kilns, highlighting the fact that you might need to slightly adjust temperatures according to the kiln that you use.


Title: Re: summary of kiln programmes for Bullseye Glass
Post by: julieHB on September 12, 2015, 08:12:09 AM
Thank you!  :)


Title: Re: summary of kiln programmes for Bullseye Glass
Post by: silkworm on September 14, 2015, 04:05:21 AM
Looks useful, thank you  :).