Title: Torching with bullseye
Post by: beadammed on June 29, 2015, 03:12:58 PM
Would I be able to melt bullseye 93 glass using my set up of a minor torch and one OxyCon?


Title: Re: Torching with bullseye
Post by: Nicknack on June 29, 2015, 03:23:00 PM
Yes, it's only a little stiffer than 104. A minor with 1 oxycon can do Boro, but not thick rods, and it does take a bit longer.

Nick


Title: Re: Torching with bullseye
Post by: beadammed on June 29, 2015, 03:26:32 PM
Thanks for that


Title: Re: Torching with bullseye
Post by: Trudi on June 30, 2015, 05:32:02 AM
you can also anneal 90 and 104 usong the same schedule!


Title: Re: Torching with bullseye
Post by: beadammed on June 30, 2015, 02:38:48 PM
Even better! I'm hoping to try some fusing and combine some Lampwork with it