Just used some Dark Silver Plum shards that I had for ages and they are lovely. I fancy having a go at making some and rummaged through the stash as remembered I had one rod labeled as DSP. The rod is opaque and from memory made a really mucky purple so thats probably why I have half a rod left!
Is there a transparent version or does it just look transparent when made into shards? Dont want to order a pack of mucky purple if its the wrong one!
It's opaque 😊
Thank you, it looks a whole lot better as a shard than solid!
Will have a go when I read up on how to!
Helen x
You can get it to go a nice metallic silver .... Great for light bulbs at Christmas!