Hi,
Are there any other Effetre colours that are as soft (or very similar) as the Opaque white?
Failing that, and CIM that is a similar softness?
Thanks
Tony
do you mean 'soft and easy to melt' or 'soft colour'? Being a bit dim here.
CIM Peace is a nice white to work with, and CIM Marshmallow is a semi-opaque white..
Effettre Pea Green is nice and soft
Effetre Ivory is very soft and Double Helix Zephyr is soft (if pricey!)
Quote from: lampworklover on June 23, 2014, 11:18:44 AM
do you mean 'soft and easy to melt' or 'soft colour'? Being a bit dim here.
CIM Peace is a nice white to work with, and CIM Marshmallow is a semi-opaque white..
Hi. I meant soft and easy to melt.
Thanks
Tony
Most Effetre opaques are soft, but white is probably the softest.