Text only
|
Text with Images
Frit-Happens !
Lampwork => COE 104 => Topic started by: the lady with the lamp on June 15, 2014, 09:58:34 PM
Title:
coe 104 enamel on 96coe glass ?
Post by:
the lady with the lamp
on
June 15, 2014, 09:58:34 PM
Hi can you use 104coe enamel on 96coe glass,i know you can use 96coe frit on 104coe glass at the 10%rule can anyone help please,thanks Parin.
Title:
Re: coe 104 enamel on 96coe glass ?
Post by:
Hamilton Taylor
on
June 16, 2014, 08:22:54 AM
Should be doable - try it and see! :)
Text only
|