Thank you all for your amazing advice.  Today I have been given a HUGE supply of float glass…..free!!!  and although I do have a basic FUSING schedule I can't seem to find a SLUMPING schedule.  Could anyone please point me in the direction of a slumping schedule.  Or do they have one they could sure with me please.  Im using an SC2 Paragon kiln and need it in oC please….but I can convert if it comes on Fahrenheit.

Thanks you all so much!!

Janey x


Title: Re: float glass
Post by: June on December 20, 2013, 02:32:35 PM
I don't use float but am sure you will find info on one of the suppliers websites or even on here if you look in the fusing boards  :)


Title: Re: float glass
Post by: lemon kitten on December 20, 2013, 03:17:12 PM
I've looked on the fusing page......in fact I've begin looking for ages.....all I can find is someone who suggested adding 20oc to the bullseye slumping schedule.  If no one can suggest anything else that's where I'll start.  :)

Janey


Title: Re: float glass
Post by: bob proulx on December 20, 2013, 04:39:27 PM
I have used the schedule at the link below and it works well.
Bob

http://glasswithapast.com/recycled-glass-firing-schedules/


Title: Re: float glass
Post by: lemon kitten on December 20, 2013, 05:31:53 PM
Bob that's great...thank you so much

Janey


Title: Re: float glass
Post by: firedinglass on December 21, 2013, 03:22:56 AM
I was just about to respond but this schedule looks great! Happy slumping" :)


Title: Re: float glass
Post by: lemon kitten on December 21, 2013, 11:19:00 AM
Whoop! Thanks Bob……..I'll start with that schedule……and tweak if needs be…thank you so much

Janey


Title: Re: float glass
Post by: Pauline on December 21, 2013, 01:47:35 PM
thanks Bob that whole website is brilliant


Title: Re: float glass
Post by: bob proulx on December 21, 2013, 04:37:20 PM
You are all welcomed. I enjoy creating with recycled glass.