Just wondered how I get fire scale off stainless steel please.
Difficult one. The traditional method is a nitric acid based pickle - and you really, really don't want that in the house.
The simple answer is to just polish back.
Yes, I had read about the nasty pickle - so I will polish :)
Thanks George