do not practice black stringer work on red bead - you can't see what the fleck you're doing!! :-\ :-\
Yep - also that terrible moment when soneone suggests "some ladybird beads"........ ;)
Quote from: Redhotsal on April 12, 2013, 12:25:16 PM
Yep - also that terrible moment when soneone suggests "some ladybird beads"........ ;)
;D ;D
;D ;D
haha, yeah I did this the other night so pleased to read I am not the only one :)
It's a nightmare to see! I decided to make a set of red beads with black and white decoration on them. Never again!
I once tried making a little demon - much the same problem ;)
The cure might be to leave the black dots raised untill the pattern is finished.
I had this issue on one bead with red, black, white and yellow dots in a special pattern. I wanted the dots in digonal rows. I got them in diagonal rows, the red and black ones in one direction and the white and yellow ones in the opposite way. I'm lucky with this (ehm) mistake for this bead.