Title: What size saw blade ?
Post by: the lady with the lamp on February 16, 2013, 12:37:44 PM
Hi,could anyone tell me what size saw blade do i need to cut copper sheet 0.9-1.2,thanks Parin.
Title: Re: What size saw blade ?
Post by: mizgeorge on February 16, 2013, 04:56:30 PM
I would use a vallorbe 2/0, but you could use a fair bit thicker - up to a 1 for the 0.9 and right up to a 4 for the 1.2.

I'm sure I've posted this somewhere before, but here's my handy dandy size guide for saw blades

(http://i149.photobucket.com/albums/s76/mizgeorge/bladesizes.jpg)
Title: Re: What size saw blade ?
Post by: the lady with the lamp on February 17, 2013, 02:43:54 PM
Thanks for the info,Parin.