I've noticed that we have a lot of newbies popping up lately (welcome all). As we have not been getting too many new threads lately I thought it would be nice to give the newbies a new year present. I wondered if we could share one or two of our top tips that we have learnt along the way. Not a whole tutorial, but snippets of things like the "top tips" that you sometimes see that really make life easier.
I'l start of with a couple as examples.
* When applying stringer always move the bead not the stringer.
* When putting bead release onto your mandrel, give it a twirl while in the pot to remove excess then tap the bottom (clean end) on your worktop to ensure a clean straight hole.
Get the idea? So what have you got?
Happy New Year everyone
Nete
I think this is a really good idea. Having been around just about a year I still think I am in the newbie group.
The tip about a tap on bottom to get a clean straight hole is new to me. ( I do hope I read that right)
My Tip
A kiln is nice but essentail when you start......advertise on here for kiln space
second tip
Spell check before you post.
I read a tip somewhere the other day that I'll pass on and that I'm try to adopt myself:
If the work on the mandrel goes wrong don't just dump it in a jar of water but stick it in the kiln (once solid again) or in the blanket or beads or whatever you use: the results might still be interesting, or a useful lesson, or at least if it's not shattered into a hundred pieces and mixed with bead release and other rubbish you could clean it up and slump it or use it in a pot melt.
Happy New Year
Quote from: Rosenquartz on January 01, 2013, 11:21:18 AM
I read a tip somewhere the other day that I'll pass on and that I'm try to adopt myself:
If the work on the mandrel goes wrong don't just dump it in a jar of water but stick it in the kiln (once solid again) or in the blanket or beads or whatever you use: the results might still be interesting, or a useful lesson, or at least if it's not shattered into a hundred pieces and mixed with bead release and other rubbish you could clean it up and slump it or use it in a pot melt.
Happy New Year
Following on from that -
However horrible a bead is, there will be someone somewhere who adores it.
I've made the most hideous monstrosities, and someone has said, "Oh,that's nice!" We don't like it because it's not what we were aiming for, but nobody else knows what we were aiming for! If it's all out of shape, they like it for its "organic quality", and if you overheated it and the middle smeared when you encased it, they like it because it's "different". One of my most admired beads is a great greeny-blue misshapen lump that was one of my first attempts at Corinna's Rainbow beads. I must try those again, but I bet that if I manage e good one, people will still prefer the other one.
Happy New Year!
Nick
Don't be afraid of Big Hole Beads...as long as you start off by really heating the mandrel it keeps the glass cooler so it's more manageable. I start my beginnners off on big hole mandrels. A bit like learning to knit with big needles!
My tip would be
always remember which is the hot end.
Mine is to mark your silver glass or any more expensive glass or intense black so that you don't mix it up with the less expensive glass (learnt the hard way - I used almost a whole rod of triton thinking it was ordinary black... :'( I thought I would remember which was which from where it was on the bench)
Brilliant idea.
My tips, as a newbie still:
1) don't be afraid to ask questions, especially here. They don't bite, well occasionally if you haven't used the search function first. Every body here was a newbie once and has been there and done it, and love to share their experience
2) take part in the competitions that go on each month. They're fun and they are now won on talent (just as well for me really)
3) you don't have to have a kiln to start with. I'm limited to small lentils and have to be careful to ensure everything stays warm, but I found a friendly local FH member who I deliver beads to once a week and she kilns them for me.
That's it for me.
I'd say:
1) Stay away from tools and rollers until you've mastered making rounds and donuts freehand first. I didn't and it then took me ages to "re-learn" the basics.
2) Don't go buying every single silver glass rod known to man until you've mastered the easier ones first (Triton, Psyche etc). You'll only waste your money.
3) If you have a frustrating time at the torch, get up and walk away. Some days/sessions are just crappy!
4) Practice making 100 spacers. This is incredibly dull but will teach you more about the way glass works than anything else you'll do.
5) Try not to compare your progress to others. Even the person who started at the same time as you could have been on their torch 12 hours a day, whilst you may only have done 2 hours a day over the same time period.
6) Buy "Passing the Flame" - it's worth it, and will teach you more than you can imagine.
7) Spend time just browing old posts on this forum. It will also teach you more than you can imagine.
Check the lids on the bead release before shaking.............
1. Try everything
2. Don't be afraid to experiment
3. If it isn't turning out the way you want it to, turn it into something else!
4. Don't beat yourself up if it turns out badly - every bit of torch time adds to your experience.
5. Same as Helbels - if you are really not 'feeling it', go and do something else.
6. If something doesn't go as planned when you first have a go, remember to go back to it further down the line, you will surprise yourself.
7. Have FUN! ;)
I'd add:
- Keep hold of your first beads and look back every now and then to see how far you've progressed.
- look at some of the earlier threads, it reminded me that everyone started somewhere and when you see the gorgeous beads people are now making it gave me hope that one day I will alos produce stunning beads - I just don't know when that one day will be ;D
You can take tea breaks - when I started I torched for hours on end without a break, thinking I would have to bleed the pipes each time I stopped... :-[ ;D
Quote from: nete on January 01, 2013, 10:46:16 AM
* When putting bead release onto your mandrel, give it a twirl while in the pot to remove excess then tap the bottom (clean end) on your worktop to ensure a clean straight hole.
I didn't know about this one, will give it a try.
Most of the ones I can think of have aleady been said except
Try to keep your mandrel and bead release hot (around the bead)- especially when using a press (tip from Astrid not me)
mine would be
tie your hair back
use a rod rest between beads so that the hot end is always at the top
check the torch nozzle every so often for glass chips etc
and never listen to the vioce in your head that tells u to pop the hot bead on the back off your hand just to see how hot it really is (i can show u the scar if u want )
* Practice the basic moves, like making dots or applying stringer. Practice them a lot. That way, when you want to make something fancier your intended design won't fail just because you couldn't get the dot or stringer in the right place.
* A tip I learned just a few months ago: when you want to try out a surface decoration, for example making raised flowers or leaves, practice making them on a glass rod first. That way you won't spend lots of time making a bead just in order to practice a decoration that'll turn out wrong the first ten or twenty (or more...) times. Making the bead can be good practice too, but I often run out of patience if I spend hours on fugly beads before I get the hang of some surface decoration.
* If you want to soften the entire bead (for example so that you can shape it), keep it in the outer part of the flame so that it heats up slowly. If you want to soften just a spot (for example to poke or melt in a dot), keep the bead near the torch so that the part you want to soften heats up quickly.
Quote from: Margram on January 01, 2013, 09:43:53 PM
You can take tea breaks - when I started I torched for hours on end without a break, thinking I would have to bleed the pipes each time I stopped... :-[ ;D
But beware... with my new set-up I have a solid copper tube coming through the wall to a shut-off valve then rubber tubing to my torch. When I had a tea break I shut off only at the torch and when I went back I noticed a distinct smell of gas and although I did a leak test (using a spray can of leak detector fluid) I could not find the source - I could only put it down to a slight leak somewhere due to the pressure in the pipes or the valve on the torch not shutting off 100%. I now try to remember to shut off at the valve at the wall for tea breaks, and at the valve on the outside of the wall for longer breaks.
More recently I fitted a carbon monoxide detector in the room and now it reminds me if I don't shut-off properly or if I don't turn on the room extractor fan. I think my detector will always be hypersensitive because it's positioned only about 6 inches down from the top corner of a sloped ceiling where all the hot air will accumulate.
Quote from: ARBeads on January 01, 2013, 04:12:21 PM
Check the lids on the bead release before shaking.............
LOL yes.... still need to get that spot on my kitchen ceiling ::)
A few from me:
1) Don't think you can "get away" without proper ventilation for a few months. You can't. You owe it to yourself to look after your lungs. You'll only get one pair. If you really really insist on working without extraction make sure you get LOTS of fresh incoming air. You'll freeze, but you won't poison yourself.
Even if you have extraction - you'll need fresh air to replace the stuff your pulling out so you may freeze either way! ::)
2) Lots of beads get stuck on the mandrel. You probably won't be able to get them off "by hand". Go and get some "mole grips" http://en.wikipedia.org/wiki/Locking_pliers and lock them onto the mandrel a few mm away from the bead. Wiggle the bead with your right hand (after a 10 minute soak in water) and hold the mandrel firmly in the mole grips with your left hand. (Swap hands if you're left handed). Your bead should come free without too much work, but you will often find wrapping an old cloth around the bead gives you a better grip on the bead. This is where you will see if your dots and stringer work has been melted in enough!
If you have broken the bead release and the glass is stuck to bare metal, I'm afraid it may never come off.
3) Stuck beads can make nice flower pot decorations! ;D
Always so practical Sal! :D
I would say:
1) Read old threads on this forum - I worked my way through pretty much all of them! It may not all mean much to start with, but you pick up all sorts of information.
2) When people say, practice, practice, practice, they mean it! You have to be prepared to get through quite a lot of glass on fuglies, so get some effetre in cheap colours to practice with. I like the 'selection packs' too, then you can try out a colour before buying lots of it.
3) For me, although I love to read about lampworking, nothing beats watching someone demonstrate a technique. That, and the opportunity to meet other lampworkers, is why I love to take classes when I can.
Although, given that I've only been doing this just over a year, I reckon I'm barely out of 'newbie' status myself :)
My addition would be:
VISIT FLAMEOFF ;D ;D ;D - Plenty demo's to see, lots of people to talk to, glass and tools to purchase, and torches to practice with if you see a technique you want to try while you remember it.... It is in April.
Well worth a visit - better if you can do both days, but even 1 day is worth it.
Oh yes - nearly forgot, never be afraid to ask that question, the only stupid question is the one that has not been asked. ;D
James M Knox
My two penneth for what it's worth would be revisit......I often look at old PCM of beads I made years ago...and then try and make them again.....only better......you'd be amazed how you've improved.
Janey x
I like that idea Janey as I'm a bit lacking in mojo atm, perhaps I'll have a go at remaking something x
talking about mojo, did you see the suggestion on http://melanie-graham.blogspot.co.uk/ for playing around with colour palettes?
My tip would be to make a support for the 'other end' of your mandrel as most newbies forget that it is important to hold the mandrel horizontally and invariably get a get a pointy end on the bead.
SO, get a small paddle marver, file off a few mm in one corner, then drill a shallow hole in it.
When you have dipped your mandrels, pinch off the last couple of milimetres, then you can easily balance the marver in your divet when twirling (without crumbling your bead release. I still use mine, especially for bigger beads
That doesnt make much sense does it? :-\
I'll post some piccies in a mo.
Also, to rejuvenate lumpy old bead release, get an old mandrel, bend one end into a little circle, stick it in your dremmel and whisk up your pot of bead release, adding boiled (cold) water until its all smoothy new again. It works fantastically well.
and also a few 'failed' beads in the pot of bead release, can help with mixing it up when it's settled out